A few of our practice dips here and there have had some lines where the film looks like it's overlapping on the part. It is nice and glassy on the water before we dip. Where is this coming from? (And yes, I know, there is still some PVA on the part :blush: )

OHW Paint - 2 day cure
Hydrogator
90 deg water
60 sec soak, two passes, 1.8 tip Air Gunsa
15 sec dwell time
Big Brain Mossy Oak Bottomland